Energy Dispersive X-ray Spectroscopy (EDS)

Energy Dispersive X-ray Spectroscopy (EDS) is an analytical capability that can be coupled with several applications including Scanning Electron Microscopy (SEM), Transmission Electron Microscopy (TEM) and Scanning Transmission Electron Microscopy (STEM).

EDS, when combined with these imaging tools, can provide elemental analysis on areas as small as nanometers in diameter. The impact of the electron beam on the sample produces x-rays that are characteristic of the elements found on the sample. With EDS, you can determine the elemental composition of individual points or map out the lateral distribution of elements from select areas.

View Application Notes down arrow

Ideal Uses for EDS Analysis Relevant Industries for EDS Analysis
  • Imaging and elemental composition of small areas
  • Identification/mapping of elements present in defects
  • Aerospace
  • Automotive
  • Biomedical/biotechnology
  • Compound Semiconductor
  • Data Storage
  • Defense
  • Displays
  • Electronics
  • Industrial Products
  • Lighting
  • Pharmaceutical 
  • Photonics
  • Polymer
  • Semiconductor
  • Solar Photovoltaics
  • Telecommunications
Strengths of EDS Analysis Limitations of EDS Analysis
  • Quick, “first look” analysis
  • Versatile, inexpensive, and widely available
  • Quantitative for some samples (flat, polished, homogeneous)
  • Semi-quantification for samples that are not flat, polished, and homogeneous
  • Size restrictions on samples
  • Samples must be vacuum compatible (not ideal for organic material)
  • Analysis (and coating) may spoil subsequent surface analysis
  • Limited sensitivity for low-Z elements

Application Notes

 

Quick Links

EDS Technical Capabilities

Signal Detected:
Characteristic x-rays

Elements Detected:
B-U

Detection Limits:
0.1 – 1 at%

Depth Resolution:
0.5 – 3 μm

Imaging/Mapping:
Yes

Lateral Resolution/Probe Size:
>=0.3 μm